Posted by Franz on Sunday, March 29, 2009 at 00:56:09 :
In Reply to: Anybody here ever Parkerized anything? posted by David Sherman on Sunday, March 29, 2009 at 00:25:53 :
Processwise parkerizing and hot bluing are the same process.
The chemistry is different in that parkerizing is done in a solution of phosphoric acid and zink that may also contain some magnesium. Generally the color will be acheived by adjusting the solution to the steel.
It definitely is NOT a rustproofing just as bluing is not a rustproofing.
Follow Ups: