Posted by David on Monday, January 05, 2004 at 7:19PM :
In Reply to: Ni-rod posted by Marty on Monday, January 05, 2004 at 1:17PM :
Ni-rod is the high nickle rod to use but you should still pre and post heat as you do with brazing. 350-400 degrees is the right temp. You need to cool it over 24 hours very slowly.