Posted by dan m [108.1.88.17] on Tuesday, April 09, 2013 at 21:24:26 :
In Reply to: Anodizing..... anyone have.. posted by Gary D [50.40.207.124] on Tuesday, April 09, 2013 at 21:08:41 :
uses sulphuric acid, dc voltage and temperature controlled bath within 2degrees. then a dye step. better to send the work out to have it done. should be a shop close by. paducah has a lot of metal finishers.