Posted by Chris Case [75.36.46.254] on Thursday, November 08, 2012 at 18:02:00 :

In Reply to: Re: I think fillers are dipped= in solder! posted by Sherman in Idaho [72.47.9.37] on Thursday, November 08, 2012 at 12:29:53 :

I know fersure modern tanks, probably back to FFPWs, are coated before welding. The resistance welding is by knurled wheels, like a continuous spot weld. Just look at a tank and note the rusty knurl lines, rest of tank gray metal. I suspect the solder vaporizes near the weld, but melts and seals a bit further away? And since there is little air near the vaporized solder, minimal oxidation occurs. Most of this would also hold true for zinc though. Tin plating works too. Tin, solder, and zinc all do LIKE to be soldered.

But now I'm thinking... weren't FFPW tanks rolled like a tin can? Then soldered? I'd go look but my only OE tank is in the attic, not under a truck.



Follow Ups:



Post a Followup

Name:
E-Mail:
Subject:
Message:
Optional Link
URL:
Title:
Optional Image Link
URL:


This board is powered by the Mr. Fong Device from Cyberarmy.com